Etching Method for the Microstructure of LTCC

Feng Yuan

Abstract


1wt% hydrochloride acid (HCl), 2wt% hydrofluoric acid (HF), 10wt% hydro nitride acid (HNO3), and 19wt% sodium hydroxide (NaOH), were used to etch the LTCC. The SEM analysis shows that the microstructure of the LTCC A6 (Ferro) can be obtained through the etching of the 19wt% sodium hydroxide. The XRD analysis confirmed that the glass phase can be selectively removed from the glass ceramics in a 19 wt% sodium hydroxide aqueous solution at room temperature after 20 hrs.


Full Text: PDF

Creative Commons License
This work is licensed under a Creative Commons Attribution 3.0 License.

Modern Applied Science   ISSN 1913-1844 (Print)   ISSN 1913-1852 (Online)

Copyright © Canadian Center of Science and Education

To make sure that you can receive messages from us, please add the 'ccsenet.org' domain to your e-mail 'safe list'. If you do not receive e-mail in your 'inbox', check your 'bulk mail' or 'junk mail' folders.